My car is fiberglass, and it turns out that there were several "loose" or "not solid" spots in the 'glass! After that, I patched some places with plastic filler and proceeded to sand the car the rest of the way - down to the light-blue gelcoat. Because I saw the paint was loose, I thought to myself "let's use a pressure washer to make short work of it." Bad idea. For those with still-good-factory finishes sand with 800 grit sandpaper (or Red Scotchbrite) and jump to the Applying Primer section. in my case, the original paint was heavily orange-peeled and flaking off in places, so it had to go. It's important to start with a clean surface. but the Harbor Freight gun isn't too bad once you clean and fix it